Structural Steels
Structural Steels offers a range of products tailored for construction and engineering applications. S355J2/S355J2G3/1.0577 is a low-carbon, high-strength structural steel suitable for various engineering uses, while 16/20MnCr5 is a manganese-chromium alloy steel commonly utilized in gear and bearing manufacturing. Each product aligns with the high standards of building and engineering requirements.
S355J2 steel/S355J2G3 steel/1.0577 steel
Material Classification
Carbon manganese, high yield non-alloy steel.
Meaning of S355J2
“S” for Structural steel; “355” for minimum yield strength of 355 MPa (≤ 16mm thickness); “J2” for 27J impact energy at -20°C (-4°F).
Weldability
Excellent; readily weldable to other weldable steel.
Core Material Properties
Good cold-forming due to low carbon equivalent; typically supplied in a normalized condition.
Chemical Composition
| C | Si | Mn | P | S | Cu | Cr | Ni |
| 0.20% | 0.55% | 1.60% | 0.025% | 0.025% | 0.55% | 0.30% | 0.30% |
Product Information
| Process | Hot rolled/forged | |
| Size | 16-1200 mm | |
| Length | Rods 6/9/12 meter, any length, customized fixed-length, multiple length | |
| Surface Condition | Black surface, Rough turned, Peeling, Grinding | |
| Heat Treatment | Normalized, Annealed, Quenching and Tempered, FP, SR | |
| Delivery Time | Within 7 days | |
| UT | SEP1921-84 D/d, EN10028-3 or ASTM A388 | |
| Stock | ≥3500 mt | |
| Size | 6mm-16mm | |
| As customers’ required, we also provide cold drawn material |
Heat Treatment
1 +A: Annealed (full/soft/spheroidizing)
2 +N: Normalized
3 +NT: Normalized and tempered
4 +QT: Quenched and tempered (water/oil)
Applications
S355J2G3 steel is a carbon manganese ,high yield non alloy steel. It is called S355 because of the average minimum yield for this material is 355 Mpa.As a structural steel,it has excellent strength and weldability.It can be readily welded to other weldable steel. For its low carbon equivalent, it possesses good cold-forming properties. S355J2G3 is generally supplied in a normalized condition.
16steel/20MnCr5 steel
Material Classification
European carburized, case hardening steel.
Primary Applications
Gears, worms, sealing bushings, and other components.
Key Features
Good hardenability and machinability; high surface hardness post heat treatment; notable low-temperature impact toughness.
Chemical Composition
| C | Mn | Si | Cr | S | P |
| 0.14-0.19% | 1.00-1.30% | 0.15-0.40% | 0.80-1.10% | low | low |
Product Information
| Process | Hot rolled/forged | |
| Size | 16-1200 mm | |
| Length | Rods 6/9/12 meter, any length, customized fixed-length, multiple length | |
| Surface Condition | Black surface, Rough turned, Peeling, Grinding | |
| Heat Treatment | Normalized, Annealed, Quenching and Tempered, FP, SR | |
| Delivery Time | Within 7 days | |
| UT | SEP1921-84 D/d, EN10028-3 or ASTM A388 | |
| Stock | ≥2000 mt | |
| Size | 6mm-16mm | |
| As customers’ required, we also provide cold drawn material |
Heat Treatment
1 +A: Annealed (full/soft/spheroidizing)
2 +N: Normalized
3 +NT: Normalized and tempered
4 +QT: Quenched and tempered (water/oil)
Applications
EN 1.7131 steel (16MnCr5 material) is an European standard carburized steel (case hardening steel) with good hardenability and machinability. For larger cross-section parts, high surface hardness and wear resistance can be obtained after heat treatment, and low-temperature impact toughness is also high.
20MnCr5 steel (1.7147 material) is an European standard carburized steel (case hardening steel) with high strength and toughness and good hardenability. The quenching deformation is small, the low temperature toughness and the machinability are good, but the welding performance is low. It’s generally used after carburizing quenching or quenching and tempering.